ASME SA213 T23 Tubes for Boilers and Superheaters
ASME SA213 / ASTM A213 Grade T23 (UNS K40712) is a seamless 2¼Cr-1.6W low-alloy steel tube strengthened with vanadium, niobium and boron. It needs 510 MPa minimum tensile and 400 MPa minimum yield strength, about double the yield of T22, so boiler designers use it for thinner, lighter waterwall, superheater and reheater tubes.
Dinesh Tube India supplies SA213 T23 seamless tubes from Mumbai as a supplier, stockist and exporter, with EN 10204 3.1 mill test certificates, and IBR certification, 3.2 or third-party inspection on request. For other grades see alloy steel tubes.
What Is SA213 T23 Tube?
T23 is a creep-strength-enhanced 2¼Cr steel. Tungsten replaces most of the molybdenum used in T22, while small additions of vanadium, niobium and boron form fine, stable carbides and nitrides. The result is a bainitic tube steel with much higher creep strength than T22 at similar cost, used mainly in modern utility and HRSG boilers.
- Grade: T23, UNS K40712 (2¼Cr-1.6W-V-Nb-B)
- Product: seamless tube only; ASTM A213 does not cover welded or ERW tube
- Condition: normalized and tempered, hot finished or cold finished
- Typical use: waterwalls, superheaters and reheaters at metal temperatures up to about 580 °C

SA213 T23 Tube Specification and Sizes
Exact OD, wall and length availability depends on the mill; confirm with your enquiry.
Common BWG Wall Thickness for T23 Tubes
SA213 T23 Chemical Composition (%)
Limits per current ASTM A213 editions. Older editions allowed N 0.030 max and B 0.0005–0.006 with no titanium requirement; the edition on the order and the mill certificate govern.
SA213 T23 Mechanical Properties
Heat Treatment and Tests
Welding T23 needs qualified procedures; follow the post-weld heat treatment required by your design code.
T23 vs T22 vs T91
For 9Cr-W tubes see T92 tubes.
Applications of SA213 T23 Tubes
How to Order SA213 T23 Tubes
Example: "ASME SA213 T23 seamless tubes, 38.1 mm OD × 5.0 mm minimum wall × 12,000 mm, 2,000 m, hot finished, hydrotest, EN 10204 3.1 + IBR." (illustrative)
Send your T23 tube RFQ to kamlesh@dineshtube-india.com, call or WhatsApp +91 83559 10913, or send an enquiry.
SA213 T23 Tubes: FAQs
What is ASME SA213 T23 tube?
SA213 T23 (UNS K40712) is a seamless low-alloy boiler and superheater tube steel with about 2¼% chromium and 1.6% tungsten, plus vanadium, niobium and boron. It was developed as a stronger alternative to T22, with roughly twice its allowable stress at typical superheater temperatures.
What is the difference between T23 and T22?
T22 is a 2¼Cr-1Mo steel. T23 replaces most of the molybdenum with tungsten and adds vanadium, niobium and boron, giving much higher creep strength (400 MPa minimum yield vs 205 MPa) and allowing thinner tube walls at the same pressure and temperature. T23 needs tighter control of welding and heat treatment.
Is T23 the same as T24 or T91?
No. T24 (K30736) is another 2¼Cr grade, strengthened with vanadium, titanium and boron instead of tungsten. T91 is a 9Cr-1Mo-V steel with higher oxidation resistance and creep strength, used at higher metal temperatures than T23.
What heat treatment does T23 tube need?
A213 requires T23 to be normalized at 1040–1080 °C and tempered at 730–800 °C as the final heat treatment. Welds are normally post-weld heat treated as required by the design code; industry experience has shown cracking problems in some unheat-treated T23 waterwall welds.
What should a T23 tube enquiry include?
State ASME SA213 or ASTM A213 T23, OD, minimum or average wall (mm or BWG), length, quantity, hot or cold finished, testing (hydrostatic or NDE), certificates (EN 10204 3.1, IBR if required) and the delivery destination.
Export Destinations for T23 Tubes
We supply SA213 T23 tubes from Mumbai within India and export to boiler makers, power and EPC projects in the Middle East, Africa, Asia, Europe and the Americas.