9Cr-1Mo-V Grade 91 Pressure Vessel Plate for High-Temperature Service
Grade 91 plate is 9Cr-1Mo-V-Nb creep-strength-enhanced ferritic steel ordered to ASTM A387 / ASME SA387 Grade 91, which is available only as Class 2 (585 – 760 MPa tensile, 415 MPa minimum yield). Plates are normalised and tempered. State Type 1 or Type 2, thickness, size and any extra tests.
Dinesh Tube India is a Mumbai supplier of A387 / SA387 Grade 91 plates, cut to size on request, with EN 10204 3.1 mill test certificates and third-party inspection on request.
What Is Grade 91 Plate and Why Is It Used?
Grade 91 is a 9% chromium, 1% molybdenum steel with controlled additions of vanadium, niobium and nitrogen. After normalising and tempering it has a tempered martensitic structure with much higher creep strength than Grade 22 (2.25Cr-1Mo), so it is used for high-temperature pressure parts in power plants and refineries where wall thickness and weight need to be reduced. It is the plate equivalent of A335 P91 pipe and A213 T91 tube. It is an alloy steel, not a stainless steel.


Which Specification, Class and Type Do You Need?
What Delivery Condition and Heat Treatment Apply?
Heat-treatment ranges per ASTM A387 for Grade 91; check the edition named in your order.
Mechanical Properties of Grade 91 Plate (Class 2)
Per ASTM A387 Class 2 for Grade 91. Hardness limits, where required, are set by the project or code specification.
Chemical Composition of Grade 91 Plate (Heat Analysis, %)
Grade 91 Type 1 per ASTM A387; Ti and Zr are also limited. Type 2 applies tighter limits on several elements. Product analysis tolerances per A20.
Sizes, Thickness and Cutting
Which Tests and Certification Apply?
Grade 91 Equivalent Grades
Equivalents are the nearest grades in other standards, not identical specifications; confirm the required standard before ordering.
Grade 91 Plate Specification
Specification
Type
Condition
Thickness
Width × Length
Strength
Extra Tests
Certification
How to Order Grade 91 Plate: RFQ Example
A complete enquiry lets us quote in one round. Replace the values with your own.
Send your Grade 91 plate RFQ in this format to kamlesh@dineshtube-india.com, call or WhatsApp +91 83559 10913, or send an enquiry.
Where Is Grade 91 Plate Used?
Other chrome-moly plates: Grade 22, Grade 11, Grade 5 and Grade 9. Grade 91 is also available as P91 pipe and T91 tube.
Grade 91 Plates: FAQs
Is P91 plate the same as A387 Grade 91?
Yes, in practice. "P91" is the ASME pipe designation (A335 P91) and "T91" the tube designation (A213 T91). The plate in the same 9Cr-1Mo-V steel is ASTM A387 / ASME SA387 Grade 91, Class 2. Order plate by the A387 / SA387 designation.
Which class is Grade 91 plate supplied in?
Grade 91 is available only as Class 2 under ASTM A387. Class 2 for Grade 91 means 585 to 760 MPa tensile strength and 415 MPa minimum yield strength.
What is the difference between Grade 91 Type 1 and Type 2?
Current editions of ASTM A387 split Grade 91 into Type 1 and Type 2. Type 2 has a more restricted chemical composition (for example on nickel, aluminium and residual elements) to improve creep resistance. State Type 1 or Type 2 in your enquiry; if not stated, check which edition and type your design code requires.
What heat treatment does Grade 91 plate need?
Grade 91 plate is normalised at 1040 to 1080 °C and tempered at 730 to 800 °C, and the plate is marked N. After fabrication and welding, post-weld heat treatment to the applicable code is required; your fabricator controls that.
Is Grade 91 a stainless steel?
No. With about 9% chromium, Grade 91 is a creep-strength-enhanced ferritic (tempered martensitic) alloy steel, not a stainless steel. It is chosen for strength at high temperature, not for corrosion resistance.
What is the difference between Grade 91 and Grade 22 plate?
Grade 22 is a 2.25Cr-1Mo steel; Grade 91 is a 9Cr-1Mo steel with vanadium, niobium and nitrogen additions. Grade 91 has much higher creep strength, so thinner sections can be used at high temperatures, but it needs tighter control of heat treatment and welding. They are not interchangeable without design approval.
Do you supply Grade 91 clad plate?
Explosion-bonded or roll-bonded clad plate with an A387 Grade 91 backing plate can be quoted on request. Give the backing plate thickness, cladding alloy and thickness, the clad plate specification (for example ASTM A264 for stainless cladding) and the bond tests required.
What should a Grade 91 plate enquiry include?
Give the specification (ASTM A387 or ASME SA387), Grade 91, Class 2, Type 1 or 2, thickness, width, length or cut size, quantity, heat-treatment condition, tests (Charpy, simulated PWHT coupons, ultrasonic testing, hardness if required), documents (EN 10204 3.1, 3.2 or third-party inspection) and the delivery date.
Export Destinations for Grade 91 Plates
We supply Grade 91 plates from Mumbai within India and export to fabricators, EPC contractors and plants in the Middle East, Africa, Asia, Europe and the Americas. Tell us your destination port when you enquire.