Stainless Steel Tubing for General Service
ASTM A269 tubes are seamless or welded austenitic stainless steel tubes for general corrosion-resisting and low- or high-temperature service. They are ordered by outside diameter and nominal wall (often in BWG or fractional inches) and are the usual standard for instrument, hydraulic, process and sampling lines.
Dinesh Tube India is a supplier, stockist and exporter of A269 tubes in TP304/304L, TP316/316L and other grades, in straight lengths or coils, with EN 10204 3.1 certificates and third-party inspection on request. For boiler and heat-exchanger duty see ASTM A249 welded tubes and our stainless steel tubes range.
A269 Tube Specification
| Item | Details |
|---|---|
| Standard | ASTM A269 / A269M (general requirements ASTM A1016) |
| Product | Seamless or welded austenitic stainless steel tubing, nominal wall |
| Size range usually furnished | 1/4 in (6.4 mm) ID and larger; wall 0.020 in (0.51 mm) and heavier. Smaller tubing: ASTM A632 |
| Common instrument sizes | 1/8, 1/4, 3/8, 1/2, 3/4 and 1 in OD; 6, 8, 10, 12, 16, 20 and 25 mm OD |
| Forms | Straight lengths, coils, U-bends on request |
| Condition | Heat treated (solution annealed); bright annealed or annealed and pickled |
| Ends | Plain, square cut and deburred; end caps |
A269 Grades and UNS Numbers
| Grade | UNS | Typical use |
|---|---|---|
| TP304 / TP304L | S30400 / S30403 | General process and water lines, instrument tubing |
| TP316 / TP316L | S31600 / S31603 | Instrument and hydraulic tubing, chloride service, offshore |
| TP317L | S31703 | Stronger acids and chemicals |
| TP321 | S32100 | Elevated-temperature service after welding |
| TP347 | S34700 | Elevated-temperature service after welding |
| TP310S | S31008 | High-temperature oxidising service |
A269 Table 1 lists many more austenitic grades; ask us for others.
Common Wall Thicknesses (BWG)
| BWG | 10 | 12 | 14 | 16 | 18 | 20 | 22 |
|---|---|---|---|---|---|---|---|
| Wall (mm) | 3.40 | 2.77 | 2.11 | 1.65 | 1.24 | 0.89 | 0.71 |
| Wall (in) | 0.134 | 0.109 | 0.083 | 0.065 | 0.049 | 0.035 | 0.028 |
A269 tubes are ordered by OD and nominal wall, not by pipe schedule. For scheduled pipe, see our stainless steel pipes to ASTM A312.
OD and Wall Tolerances
| Outside diameter | OD tolerance | Wall tolerance |
|---|---|---|
| Up to 1/2 in (12.7 mm) | ±0.005 in (0.13 mm) | ±15% |
| 1/2 to 1½ in (12.7 to 38.1 mm), excl. | ±0.005 in (0.13 mm) | ±10% |
| 1½ to 3½ in (38.1 to 88.9 mm), excl. | ±0.010 in (0.25 mm) | ±10% |
| 3½ to 5½ in (88.9 to 139.7 mm), excl. | ±0.015 in (0.38 mm) | ±10% |
| 5½ to 8 in (139.7 to 203.2 mm), excl. | ±0.030 in (0.76 mm) | ±10% |
| 8 to 12 in (203.2 to 304.8 mm), excl. | ±0.040 in (1.02 mm) | ±10% |
Thin-wall tubes and walls of 3/4 in and over, or with ID 60% or less of OD, have wider tolerances under A269. Check the edition on your order.
Chemical Composition (%), Common A269 Grades
| Grade | C max | Mn max | P max | S max | Si max | Cr | Ni | Mo |
|---|---|---|---|---|---|---|---|---|
| TP304 | 0.08 | 2.00 | 0.045 | 0.030 | 1.00 | 18.0–20.0 | 8.0–11.0 | – |
| TP304L | 0.035* | 2.00 | 0.045 | 0.030 | 1.00 | 18.0–20.0 | 8.0–12.0 | – |
| TP316 | 0.08 | 2.00 | 0.045 | 0.030 | 1.00 | 16.0–18.0 | 10.0–14.0 | 2.00–3.00 |
| TP316L | 0.035* | 2.00 | 0.045 | 0.030 | 1.00 | 16.0–18.0 | 10.0–14.0 | 2.00–3.00 |
*A carbon maximum of 0.040% is allowed for L grades in small-diameter or thin-wall tubing that needs many drawing passes. Other grades follow A269 Table 1; the mill certificate governs.
Mechanical Requirements: Hardness, Not Tensile
ASTM A269 has no tensile, yield or elongation requirement. Mechanical acceptance is by hardness and by the flare, flange and reverse-flattening tests below.
| Grades | Hardness max |
|---|---|
| TP304, TP304L, TP316, TP316L, TP317L, TP321, TP347, TP310S and similar austenitic grades | 90 HRB / 192 HBW |
| Higher-strength grades (for example nitrogen-strengthened XM grades) | Higher limits per A269 |
If you need guaranteed tensile properties, order to ASTM A213 (seamless) or A249 (welded), or add tension testing by agreement.
Manufacture and Heat Treatment
- Made by the seamless or welded process; welded tubing is made by an automatic process without filler metal.
- All tubing is supplied heat treated: solution annealed at 1040 °C (1900 °F) minimum for the common grades, then quenched in water or rapidly cooled.
- Bright annealing in a protective atmosphere, or annealing followed by pickling.
Required Tests
- Flaring test on seamless tubes
- Flange test on welded tubes
- Reverse flattening test on welded tubes
- Hardness test per lot
- Hydrostatic or nondestructive electric test on every tube
- Optional: intergranular corrosion test (A262), PMI, surface-finish limits and third-party inspection
A269 vs A213 vs A249
| Point | ASTM A269 | ASTM A213 | ASTM A249 |
|---|---|---|---|
| Process | Seamless or welded | Seamless | Welded |
| Intended use | General service, instrument, hydraulic and process lines | Boilers, superheaters, heat exchangers | Boilers, superheaters, heat exchangers, condensers |
| Tensile test | Not required | Required | Required |
| Other tests | Hardness, flare/flange, reverse flattening, hydro/NDE | Flattening, flaring, hardness, hydro/NDE | Flattening, flange, reverse bend, hardness, hydro/NDE |
| Wall basis | Nominal | Minimum or average, as ordered | Nominal |
Applications
- Instrumentation and impulse lines with compression fittings
- Hydraulic and pneumatic control lines, offshore and onshore
- Chemical-injection, sampling and analyser lines
- Process and transfer lines in chemical, food and pharmaceutical plants
- Low-temperature and high-temperature general service
How to Order A269 Tubes
State the specification (ASTM A269 and edition), seamless or welded, grade (or dual grade), OD, nominal wall (mm, inch or BWG), length or coil, quantity, finish, any hardness limit for compression fittings, optional tests, certification and delivery location.
Need A269 tubes? Send your tube list to kamlesh@dineshtube-india.com or call +91 83559 10913. You can also send an enquiry.
Related Products
Stainless steel tubes, ASTM A249 welded tubes, heat exchanger tubes, SS 316 small-diameter tubes, stainless steel pipes and all stainless steel products.
ASTM A269 Tubes: FAQs
What is ASTM A269?
ASTM A269/A269M is the standard specification for seamless and welded austenitic stainless steel tubing for general service. It covers nominal-wall tubing for general corrosion-resisting and low- or high-temperature service, such as instrument, hydraulic, process and transfer lines.
Does ASTM A269 have tensile strength requirements?
No. A269 does not require a tension test. Its mechanical tests are flaring (seamless), flange (welded), reverse flattening (welded) and hardness, plus a hydrostatic or nondestructive electric test on every tube. If you need guaranteed tensile values, order to A213 or A249, or add tensile testing to the order by agreement.
What sizes does A269 cover?
Tubing usually furnished to A269 is 1/4 in (6.4 mm) inside diameter and larger, with nominal walls of 0.020 in (0.51 mm) and heavier. Smaller-diameter tubing is covered by ASTM A632. Instrument tubing is most often 1/8 to 1 in or 6 to 25 mm OD.
What is the difference between A269 and A213?
A213 is for seamless boiler, superheater and heat-exchanger tubes and includes tension, flattening, flaring and hardness tests. A269 covers seamless and welded tubing for general service with lighter testing and no tensile requirement. Instrument tubing is often dual certified A269/A213.
Which grades are most common to A269?
TP304/304L and TP316/316L, often dual certified, are by far the most common. TP316L is the usual choice for instrument and hydraulic tubing with compression fittings. TP321, TP347 and TP317L are supplied for higher temperatures or stronger chemicals.
What hardness is required for A269 tubes used with compression fittings?
A269 limits hardness to 90 HRB (192 HBW) for the common austenitic grades. Many fitting makers recommend softer tube, often 80 HRB maximum, for reliable compression-fitting seals; this can be specified on the order.