This page summarises the requirements of ASME SA178 / ASTM A178, Electric-Resistance-Welded Carbon Steel and Carbon-Manganese Steel Boiler and Superheater Tubes, for Grades A, C and D. ASME SA178 is identical to ASTM A178 and is used for ASME and IBR boiler work. Always check the edition named in your purchase order.
To buy tubes, see our ASME SA178 carbon steel tubes page. A printable version is available as the ASTM A178 tube specification sheet (PDF).
Scope of SA178
| Item | Requirement |
|---|---|
| Title | Electric-resistance-welded carbon steel and carbon-manganese steel boiler and superheater tubes |
| Product | Minimum-wall-thickness ERW tubes for boiler tubes, boiler flues, superheater flues and safe ends |
| Grades | A (low-carbon), C (medium-carbon), D (carbon-manganese) |
| Sizes usually furnished | 1/2 to 5 in (12.7 to 127 mm) OD; 0.035 to 0.360 in (0.9 to 9.1 mm) minimum wall |
| Other sizes | May be furnished if they meet all other requirements of the specification |
| Safe ends | Grades C and D are not suitable for safe-ending by forge welding |
| General requirements | ASTM A450 / ASME SA450 |
| Units | Inch-pound unless the A178M (SI) designation is ordered |

Manufacture and Heat Treatment
SA178 Chemical Composition (%)
Supplying an alloy grade that requires elements not listed is not permitted when a carbon steel grade is ordered.
SA178 Mechanical Properties
For longitudinal strip tests on Grades C and D, 1.50 percentage points are deducted for each 0.8 mm (1/32 in) decrease in wall below 8 mm (5/16 in). Grade A has no tensile requirement in A178; its acceptance is by the flattening, flange and crush tests.
Dimensional Tolerances (ASTM A450, Welded Tubes)
Wall thickness: SA178 is ordered on minimum wall; the A450 tolerance for welded tubes is +18% / −0.
Values from ASTM A450; check the edition on your order.
Required Tests
IBR (Form III-B) certification and third-party inspection can be added by agreement.
Related Tube Grades
Ordering Information
An SA178 order should state: quantity; name of material (electric-resistance-welded tubes); grade (A, C or D); size (OD and minimum wall); length (specific or random); optional requirements such as product analysis or the crush test; certificates (EN 10204 3.1, IBR Form III-B or as required); and any supplementary requirements.
Need SA178 tubes? Send your grade, OD, minimum wall, length and quantity to kamlesh@dineshtube-india.com or call +91 83559 10913, or see the SA178 tubes product page.
SA178 Specification: FAQs
What does the SA178 specification cover?
ASME SA178 (identical to ASTM A178) covers minimum-wall-thickness, electric-resistance-welded carbon steel and carbon-manganese steel tubes for boiler tubes, boiler flues, superheater flues and safe ends. It has three grades: A, C and D. Sizes usually furnished are 1/2 to 5 in (12.7 to 127 mm) OD and 0.035 to 0.360 in (0.9 to 9.1 mm) minimum wall.
What is the difference between SA178 Grade A, C and D?
Grade A is low-carbon steel (0.06–0.18% C) with no tensile requirement. Grade C is medium-carbon steel (0.35% C max) with 415 MPa (60 ksi) tensile and 255 MPa (37 ksi) yield. Grade D is a killed carbon-manganese steel (1.00–1.50% Mn, 0.10% Si min) with 485 MPa (70 ksi) tensile and 275 MPa (40 ksi) yield.
Is SA178 tube seamless?
No. SA178 tubes are always electric-resistance welded and then heat treated. For seamless carbon steel boiler tubes, order SA192 (low carbon) or SA210 (medium carbon).
What heat treatment does SA178 require?
After welding, every tube is heat treated at 900 °C (1650 °F) or higher and cooled in air or in the cooling chamber of a controlled-atmosphere furnace. Cold-drawn tubes are heat treated after the final cold-draw pass at 650 °C (1200 °F) or higher.
Can SA178 Grade C or D tubes be used for safe ends?
Grades C and D are not suitable for safe-ending by forge welding. Grade A is the grade used where forge-welded safe ends are needed.
How are SA178 tolerances specified?
Dimensional tolerances come from ASTM A450 / ASME SA450 for welded tubes. SA178 is a minimum-wall specification, so the wall may be over the ordered minimum (up to +18% for welded tube) but not under it.