This page summarises the requirements of ASTM A423 / ASME SA423, Seamless and Electric-Welded Low-Alloy Steel Tubes, with the focus on Grade 1, the copper-chromium-nickel-phosphorus (Corten-type) grade used for air preheater and economiser tubes. Grades 2 and 3 are shown for comparison. Always check the edition named in your purchase order.
To buy tubes, see our ASTM A423 Grade 1 tubes page. A printable version is available as the ASTM A423 Grade 1 tube specification sheet (PDF).
Scope of ASTM A423
| Item | Requirement |
|---|---|
| Title | Seamless and electric-welded low-alloy steel tubes |
| Product | Minimum-wall-thickness tubes for pressure-containing parts such as economisers, and other uses where corrosion resistance is important |
| Grades | 1 (Cu-Cr-Ni-P), 2 (Ni-Cu-Mo, low P), 3 (Cu-Ni-Sb, low C) |
| Types | Seamless or electric-resistance welded (ERW) |
| Manufacture finish | Hot finished or cold finished |
| Sizes usually furnished | 1/2 to 5 in (12.7 to 127 mm) OD; 0.035 to 0.500 in (0.9 to 12.7 mm) minimum wall |
| Other sizes | May be furnished if they meet all other requirements of the specification |
| Mechanical properties | Do not apply to tubing under 1/4 in (3.2 mm) ID or 0.015 in (0.4 mm) wall |
| General requirements | ASTM A450 / ASME SA450 |

Manufacture and Heat Treatment
A423 Chemical Composition (%)
Heat analysis limits. Grade 1’s deliberately high phosphorus, with copper and chromium, gives its resistance to atmospheric and acid dew-point corrosion.
A423 Mechanical Properties
For longitudinal strip tests, 1.25 percentage points are deducted from the elongation for each 0.8 mm (1/32 in) decrease in wall below 8 mm (5/16 in).
Dimensional Tolerances (ASTM A450)
Wall thickness: A423 is ordered on minimum wall, so the wall may be over the ordered minimum but not under it. Under A450 the plus tolerance is +18% for welded tubes; +20% (up to 1½ in OD) or +22% (larger) for cold-finished seamless tubes; and larger for hot-finished seamless tubes, depending on size.
Values from ASTM A450; check the edition on your order. Hot-finished seamless tubes have wider OD tolerances.
Required Tests
EN 10204 3.1 certificates are standard; 3.2 certificates, IBR and third-party inspection can be added by agreement.
Related Tube Grades
Ordering Information
An A423 order should state: quantity; type (seamless or electric-resistance welded); grade (1, 2 or 3); manufacture (hot finished or cold finished); size (OD and minimum wall); length (specific or random); optional requirements such as product analysis or the supplementary NDE requirement; certificates (EN 10204 3.1, IBR or as required); and the specification number and edition.
Need A423 Grade 1 tubes? Send the type, OD, minimum wall, length and quantity to kamlesh@dineshtube-india.com or call +91 83559 10913, or see the A423 Grade 1 tubes product page.
ASTM A423 Specification: FAQs
What does the ASTM A423 specification cover?
ASTM A423 / ASME SA423 covers minimum-wall-thickness, seamless and electric-resistance-welded low-alloy steel tubes for pressure-containing parts such as economisers, and other uses where corrosion resistance is important. Sizes usually furnished are 1/2 to 5 in (12.7 to 127 mm) OD and 0.035 to 0.500 in (0.9 to 12.7 mm) minimum wall.
What is the chemical composition of A423 Grade 1?
Carbon 0.15% max, manganese 0.55% max, phosphorus 0.06–0.16%, sulphur 0.060% max, silicon 0.10% min, copper 0.20–0.60%, chromium 0.24–1.31% and nickel 0.20–0.70%.
What are the mechanical properties of A423 Grade 1?
Minimum tensile strength 415 MPa (60 ksi), minimum yield strength 255 MPa (37 ksi) and minimum elongation 25% in 50 mm. Grade 2 has the same tensile limits; Grade 3 requires 380 MPa tensile, 230 MPa yield and 35% elongation.
What heat treatment does A423 require?
All tubes are normalised, or given whatever heat treatment is needed to meet the specification. Tubes may be hot finished or cold finished.
Which tests are required by A423?
Tension, flattening, flaring (seamless) or flange (welded), reverse flattening (welded) and hardness tests, plus a hydrostatic or non-destructive electric test on every tube. The tubes must also stand expanding and bending without cracking.
Is A423 Grade 1 the same as Corten?
Grade 1 uses the same copper-chromium-nickel-phosphorus alloying idea as Corten A weathering steel, so it is often called Corten tube. Corten is a trade name for plate and sheet; tubes for air preheaters and economisers are ordered to ASTM A423 / ASME SA423.